QuesTek titanium alloy to be tested by Norsk for strength 15% higher than Ti6Al4V

July 26, 2018
Source: ASM International

Norsk Titanium, Plattsburgh, N.Y., , and QuesTek Innovations LLC, Evanston, Ill., announce a collaborative effort to test novel titanium alloys for applicability in additive manufacturing processes. As part of this collaboration, the companies are evaluating a QuesTek-designed titanium alloy using Norsk’s Rapid Plasma Deposition (RPD) process. Preliminary evaluation of the alloy is complete and Norsk has manufactured initial test specimens.

The test program will characterize the alloy microstructure, provide initial material properties, and will confirm QuesTek’s titanium alloy performance using Norsk’s proven production process. QuesTek’s patented titanium alloy has previously demonstrated approximately 15% greater strength and improved ductility over traditional Ti-6Al-4V in both wire-based Electron Beam Additive Manufacturing and in traditional casting processes.

“Based on our interactions with the major aerospace component suppliers and aircraft OEMs in the United States, Europe and Japan, we know there is a significant need for reliable, higher performance Additive Manufactured titanium components that will enable light weighting and an increase in component life,” said QuesTek’s Manager of Business Development, Jeff Grabowski.

When implemented, the new alloy is expected to provide material properties in excess of the standard Ti-6Al-4V already provided by Norsk.

“QuesTek’s novel titanium alloy will allow RPD to grow into new applications and will allow designers to take further advantage of the benefits of additive processes,” says Norsk Vice President Nicholas Mayer.

The patented Rapid Plasma Deposition process transforms titanium wire into complex components suitable for structural and safety-critical applications. RPD is the world’s first FAA-approved, 3D-printed, structural titanium, delivering substantial lead-time and cost savings for aerospace, defense, and commercial customers.

www.norsktitanium.com

www.questek.com 