Solar Atmospheres develops better cleaning process for vacuum furnace heat exchangers

October 12, 2018
Source:

Solar Atmospheres, Souderton, Pa., announces that it has developed an improved process to clean heat exchanger fins that have become clogged with dirt and debris.

In the operation of vacuum furnaces, the quench gas heat exchanger fins can become clogged with various debris and dirt that is very difficult to completely clean with standard pressure washing and other conventional methods. The clogged heat exchanger greatly impedes quench gas flow, resulting in reduced work cooling rates.

 

Solar’s special process involves a 12-hour soak submerged in a suitable tub using a water base cleaning agent. Recirculated forced water jets wash out the accumulated dirt from deep inside the heat exchanger. It is then pressure washed and blown dry with nitrogen gas. The heat exchanger is cleaned to an as new condition and then returned to the user.

 

www.vacpumpservices.com, an affiliate of Solar Atmospheres.

 

Solar Atmospheres, Souderton, Pa., announces that it has developed an improved process to clean heat exchanger fins that have become clogged with dirt and debris.

In the operation of vacuum furnaces, the quench gas heat exchanger fins can become clogged with various debris and dirt that is very difficult to completely clean with standard pressure washing and other conventional methods. The clogged heat exchanger greatly impedes quench gas flow, resulting in reduced work cooling rates.

 

Solar’s special process involves a 12-hour soak submerged in a suitable tub using a water base cleaning agent. Recirculated forced water jets wash out the accumulated dirt from deep inside the heat exchanger. It is then pressure washed and blown dry with nitrogen gas. The heat exchanger is cleaned to an as new condition and then returned to the user.

 

www.vacpumpservices.com, an affiliate of Solar Atmospheres.

 