Heat Treat 2019 paper abstract: The Future of the Integral Quench Furnace

June 26, 2019
Source:

A presentation by Seco Vacuum, Seco Warwick, and the Herring Group covers progress in carburizing technology, in which atmosphere gas and low-pressure vacuum carburizing are well known, well-established, and distinct processes.

 

However, rarely do these two technologies compete in the same commercial space. Gas carburizing in integral (sealed) oil quench furnaces is the workhorse of the industry, while low-pressure carburizing produces the absolute best quality. Combining the best of both methods will result in a more competitive future!

 

The changing workforce and the demand for global competitiveness in manufacturing are the motivating factors behind combining the best of both atmosphere and vacuum carburizing technology into a single piece of equipment whose total cost of ownership makes the technology competitive.

 

Engineers have been struggling for years to find an alternative to the use of endothermic gas and/or nitrogen-methanol system to create and control a carrier gas atmosphere. The future demands that no endothermic gas be used.

 

After several years of research, a practical solution has emerged, been tested, and deployed. This paper provides some of the extensive results, features, motivation, and plans for the next generation of integral quench furnaces.

 

Heat Treat 19, Detroit, Mich.

Tuesday, October 15, 2019: 9:40 AM

 

Mr. Mark Hemsath, Seco Vacuum Technologies LLC, Meadville, Pa. www.secovacusa.com

 

Prof. Daniel H. Herring , The Herring Group Inc., Elmhurst, Ill. www.heat-treat-doctor.com

 

Mr. Tomasz Przygonski, Seco Warwick S.A., Swiebodzin, Polandwww.secowarwick.com

 

https://www.asminternational.org/web/heat-treat-2019

 

A presentation by Seco Vacuum, Seco Warwick, and the Herring Group covers progress in carburizing technology, in which atmosphere gas and low-pressure vacuum carburizing are well known, well-established, and distinct processes.

 

However, rarely do these two technologies compete in the same commercial space. Gas carburizing in integral (sealed) oil quench furnaces is the workhorse of the industry, while low-pressure carburizing produces the absolute best quality. Combining the best of both methods will result in a more competitive future!

 

The changing workforce and the demand for global competitiveness in manufacturing are the motivating factors behind combining the best of both atmosphere and vacuum carburizing technology into a single piece of equipment whose total cost of ownership makes the technology competitive.

 

Engineers have been struggling for years to find an alternative to the use of endothermic gas and/or nitrogen-methanol system to create and control a carrier gas atmosphere. The future demands that no endothermic gas be used.

 

After several years of research, a practical solution has emerged, been tested, and deployed. This paper provides some of the extensive results, features, motivation, and plans for the next generation of integral quench furnaces.

 

Heat Treat 19, Detroit, Mich.

Tuesday, October 15, 2019: 9:40 AM

 

Mr. Mark Hemsath, Seco Vacuum Technologies LLC, Meadville, Pa. www.secovacusa.com

 

Prof. Daniel H. Herring , The Herring Group Inc., Elmhurst, Ill. www.heat-treat-doctor.com

 

Mr. Tomasz Przygonski, Seco Warwick S.A., Swiebodzin, Polandwww.secowarwick.com

 

https://www.asminternational.org/web/heat-treat-2019

 