Nitrex Metal studies influence of standard deviations on nitriding, ferritic nitrocarburizing

October 7, 2019
Source:

Jack Kalucki, Nitrex Metal Inc., Montreal, Quebec, discusses how standard allowed deviations in control parameters affect actual results in controlled nitriding and ferritic nitrocarburizing, in a presentation at Heat Treat 2019. These technologies have become commonly used to improve wear resistance, mechanical properties, and corrosion resistance. The framework for process control is based on standards such as AMS 2759/10 and 2759/12A. In all cases, these standards allow for a tolerance in control parameters.

 

This work presents the influence of standard allowed deviations in control parameters, for example, nitriding potential and temperature for a given furnace class, on actual results when comparing Iron, carbon steel, 4140, and H13 samples. Comparative results point to interesting variations in white layer thickness.

 

We also discuss other potential factors such as the shift of actual results due to carbon and alloying elements, and the subsequent alteration of results between expected and actual as demonstrated by shifting boundaries on the Lehrer diagram.

 

As a conclusion, the study underlines the fact that while tolerances are allowed, precise control in specific furnace classes is necessary to obtain an ideal repetition of results. Additionally, improved control lowers gas usage and gas flows to a strict minimum, with a direct impact on the cost of quality, cost of treatment, and emissions affecting the environment.

 

Title: “How Does Precise Control Affect the Outcome of Nitriding and Ferritic Nitrocarburizing Cycles?”

Jack Kalucki, Nitrex Metal Inc., Montreal, Quebec

 

Tuesday, October 15, 2019: 11:00 AM

251A (TCF Center), Detroit

https://www.asminternational.org/web/heat-treat-2019

 

Jack Kalucki, Nitrex Metal Inc., Montreal, Quebec, discusses how standard allowed deviations in control parameters affect actual results in controlled nitriding and ferritic nitrocarburizing, in a presentation at Heat Treat 2019. These technologies have become commonly used to improve wear resistance, mechanical properties, and corrosion resistance. The framework for process control is based on standards such as AMS 2759/10 and 2759/12A. In all cases, these standards allow for a tolerance in control parameters.

 

This work presents the influence of standard allowed deviations in control parameters, for example, nitriding potential and temperature for a given furnace class, on actual results when comparing Iron, carbon steel, 4140, and H13 samples. Comparative results point to interesting variations in white layer thickness.

 

We also discuss other potential factors such as the shift of actual results due to carbon and alloying elements, and the subsequent alteration of results between expected and actual as demonstrated by shifting boundaries on the Lehrer diagram.

 

As a conclusion, the study underlines the fact that while tolerances are allowed, precise control in specific furnace classes is necessary to obtain an ideal repetition of results. Additionally, improved control lowers gas usage and gas flows to a strict minimum, with a direct impact on the cost of quality, cost of treatment, and emissions affecting the environment.

 

Title: “How Does Precise Control Affect the Outcome of Nitriding and Ferritic Nitrocarburizing Cycles?”

Jack Kalucki, Nitrex Metal Inc., Montreal, Quebec

 

Tuesday, October 15, 2019: 11:00 AM

251A (TCF Center), Detroit

https://www.asminternational.org/web/heat-treat-2019

 