NanoAL brings Addalloy to Mitsubishi

May 29, 2021
Source: ASM International

NanoAL LLC, Boston has signed a commercial license agreement with Mitsubishi Corp. RtM Japan Ltd. to bring its Addalloy family of advanced aluminum alloy powders to the metal additive manufacturing market in Asia.

The companies also signed a letter of intent for potential partnerships on additional NanoAL advanced aluminum alloy products including aluminum casting and rolled sheets for automotive and other industrial applications. Addalloy is an aluminum alloy technology designed and developed for metal additive manufacturing via laser powder bed fusion. It consists of 5T, 7S, and HX compositions, each with application-specific performance levels tailored to the demands of automotive, motorsports, aerospace, and industrial markets.

Addalloy powders work on major laser-based OEM platforms for metal 3D printing including EOS, SLM Solutions, Renishaw, Concept Laser, and many others. 