Title: |
Magnesium AZ31B-H24 Alloy Sheet: Tensile Test Data |
|
Abstract: |
This data set contains engineering and true stress-strain data obtained experimentally from commercial Mg AZ31B rolled sheet supplied in the H24 temper. Details on composition, test specimen preparation, and test setup are provided in the data file. Tensile tests were conducted until rupture at temperatures from 50 to 450°C (in increments of 50°C) for strain rates of 10-3 and 10-1 s-1. Load was measured by a load cell in-line with the load train while displacement was recorded using a linear variable differential transformer connected to a hydraulic piston that drives the test frame. All calculations and conversions are described in the linked source paper. |
|
Authors/contributors: |
Principal investigators: Eric Taleff, University of Texas at Austin, Austin, TX, USA; Aravindha R. Antoniswamy, Intel Corp., Chandler, AZ, USA. |
|
Publication date: |
2022-01-01 |
|
Sponsoring organization(s): |
National Science Foundation, Washington, DC; General Motors Co., Warren, MI, USA. |
|
Keywords: |
Alloy AZ31B-H24, engineering stress-strain data, magnesium alloy sheet, tensile testing data, true stress-strain data |
|
Subject tags: |
2526 (Magnesium-aluminum-zinc alloys) 2270 (Sheets and strips) 3921 (Strain rate) 4002 (Temperature) 3943 (Tensile properties) 3925 (True strain) 265 (Uniaxial tension testing) |
|
Related content: |
A.R. Antoniswamya, E.M. Taleff, L.G. Hector, Jr., J.T Carter, Plastic deformation and ductility of magnesium AZ31B-H24 alloy sheet from 22 to 450 °C, Materials Science and Engineering: A, 631 (2015) 1-9. https://doi.org/10.1016/j.msea.2015.02.018 |
|
License: |
Distributed by ASM International. All rights reserved. Use is subject to terms and conditions. |
|
Data set format: |
Structured data are saved in two Excel workbooks corresponding to two strain rates used for testing. File size is approximately 60 MB for the 0.1 s-1 strain rate data and 45 MB for the 0.001 s-1 strain rate data. |