AK 420 martensitic stainless steel has good corrosion resistance with increased strength over other 400 martensitic stainless steels. The alloy is magnetic.

  • From:

    Alloy Digest, Stainless Steel Collection 2011-Present

  • Publisher: ASM International
  • Published: June 01, 2015
  • Pages: 2