Carbon-Iron-Nickel Ternary Alloy Phase Diagram (based on 1973 Sharma R.C.)

Author: Sharma R.C.; Kirkaldy J.S.   |   Document Download   |   Product code: ZAPD-C-FE-NI-1100831

File size: 504 KB

Classified as: Batteries and Energy Storage Binary Systems ...more

Free to Members

Diagram Type: ternary, isothermal section

Concentration range: partial composition; Fe-Fe92Ni8-C10Fe82Ni8-C10Fe90

Temperature: 730.0 - 730.0 °C

Nature of investigation: calculated

Source: ASM Alloy Phase Diagrams Center, 2007; data from Sharma R.C., Thermodynamics and kinetics of the proeutectoid ferrite reaction in Fe-C-Ni in the vicinity of 730 ┬░C, Can. Metall. Q., Vol. 12, 1973, p 391-401

Reviewed under the auspices of the Alloy Phase Diagram International Commission.

Document includes crystal data for the Carbon-Iron-Nickel system, allotropic transformation data, and related references.