Carbon-Uranium Binary Alloy Phase Diagram (based on 1972 Collot C.)

Author: Collot C.; Couterne A.; Guillaume C.; Giraud Heraud F.; Guillaumin J.   |   Document Download   |   Product code: ZAPD-C-U-905266

File size: 481 KB

Classified as: Batteries and Energy Storage Binary Systems ...more

Free to Members

Diagram Type: binary phase diagram

Concentration range: partial composition; 99.975-100 at.% U

Temperature: 600.0 - 1400.0 °C

Nature of investigation: experimental

Source: ASM Alloy Phase Diagrams Center, 2007; data from Collot C., ETUDE DES TRANSFORMATIONS DE PHASE DANS LES ALLIAGES URANIUM-VANADIUM. INFLUENCE DE LA TENEUR EN CARBONE, J. Nucl. Mater., Vol. 43, 1972, p 28-50

Reviewed under the auspices of the Alloy Phase Diagram International Commission.

Element concentrations are presented in atomic percent.

Document includes crystal data for the Carbon-Uranium system, allotropic transformation data, and related references.