MAGNESIUM EZ33A: Magnesium casting alloy

Author: n/a   |   Document Download   |   Product code: ZMG65

File size: 150 KB

Classified as: Magnesium

Free to Members
Material Data Sheet for MAGNESIUM EZ33A, a Cast magnesium-rare earth, including information regarding Compressive, Fatigue, Tensile, High temperature, Hardness, Density or mass, Thermal, Electrical, Chemical composition, Machining, Welding or joining, Heat treating, Casting.
  • From: Alloy Digest, Magnesium Collection (ASM International)
  • Published: May 01, 1968
  • Pages: 2