Carbon Steel and C-Mn Steel: Influence of Plastic Deformation on Transformation

Author: Edited by G. Vander Voort   |   Document Download   |   Product code: ZTTTI598B

File size: 455 KB

Classified as: Carbon and Alloy Steels

Free to Members
Time-Temperature Curve for Fe-0.105C-1.53Mn, a High-manganese carbon steel; a Nonresulfurized carbon steel, including information regarding Chemical composition, Microstructure, Heat treating.
  • From: Atlas of Time-Temperature Diagrams for Irons and Steels (ASM International)
  • Published: January 01, 1991
  • Pages: 1