2124 Al-15% SiCp (VHP)

Published: 2015

Metal matrix composites with discontinuously dispersed reinforcements have been developed to achieve improvement in specific stiffness for applications in aerospace and automobile structures.

Material Resources / Publications

Other Formats Available:

Al-4Li (UL40)

Published: 2015

Commercial Al alloys with high Li contents (>2.5 wt.%) are generally produced by spray forming since conventional DC casting caused hot tearing in the ingots and melt spinning results in heavy oxidation.

Material Resources / Publications

Other Formats Available:

Al-3.2Cu-1.6Li

Published: 2015

Al–Li alloys have high specific stiffness and are being considered for structural members in aerospace industries.

Material Resources / Publications

Other Formats Available:

Al-B4C

Published: 2015

Boron carbide (B4C) is a covalently bonded ceramic material being used as a reinforcement because of its high hardness along with high chemical and wear resistance.

Material Resources / Publications

Other Formats Available:

7075 Al Alloy

Published: 2015

7075 Al alloy is a precipitation hardenable alloy and is used for various aerospace applications.

Material Resources / Publications

Other Formats Available:

7020 Al Alloy

Published: 2015

7020 Al alloy is heat treatable wrought aluminum alloy used for aerospace structural components.

Material Resources / Publications

Other Formats Available:

6951 Al Alloy

Published: 2015

6951 Al alloy is a Al-Mg-Si based system and is used as forgings and extrusions.

Material Resources / Publications

Other Formats Available:

7085 Al Alloy

Published: 2015

Al 7085 is a high strength heat treatable alloy which is used as rolled stock for aerospace applications.

Material Resources / Publications

Other Formats Available:

7075 Al Alloy + Mn

Published: 2015

7075 Al alloy was modified by the addition of manganese.

Material Resources / Publications

Other Formats Available:

8090 Al Alloy (Low Li)

Published: 2015

In 8090 grade Al-Li alloy, the lithium content is in the range 2.2-2.7%. In this study, the influence of lowering the lithium content to 1.85% on the hot deformation characteristics of the alloy is investigated.

Material Resources / Publications