8090 Al Alloy

Published: 2015

Al-Li-Cu-Mg alloys belong to 8090 grade and are light weight, high stiffness, newer alloys being developed for aircraft structural applications.

Material Resources / Publications

Other Formats Available:

8090 Al Alloy + Be

Published: 2015

In aluminum alloys, trace additions have significant influence on the kinetics of precipitation and stress-corrosion properties. Beryllium additions are considered to be beneficial.

Material Resources / Publications

Other Formats Available:

6061 Al Alloy

Published: 2015

6XXX Al alloys are extensively used for extruded sections and are heat treatable.

Material Resources / Publications

Other Formats Available:

4043 Al Alloy

Published: 2015

4043 Al alloy has silicon particles in aluminum matrix and is a forgeable alloy.

Material Resources / Publications

Other Formats Available:

3003 Al Alloy

Published: 2015

Al alloy 3003 contains Si, Fe and Mn which form intermetallic particles that get distributed in the matrix since they are insoluble in Al.

Material Resources / Publications

Other Formats Available:

5556 Al Alloy

Published: 2015

Aluminum alloy 5556 is essentially Al-Mg-Mn alloy which finds application as welding electrodes.

Material Resources / Publications

Other Formats Available:

6201 Al Alloy

Published: 2015

6201 aluminum alloy is used for all aluminum alloy conductors (AAAC) which replace steel reinforced aluminum conductors (ACSR).

Material Resources / Publications

Other Formats Available:

6063 Al Alloy

Published: 2015

6000 series of Al alloys contain additions of Mg and Si and are commonly used for extrusions in view of their excellent extrudability and heat treatability .

Material Resources / Publications

Other Formats Available:

6351 Al Alloy

Published: 2015

Al 6351 is a Al-Mg-Si alloy which is heat treatable by precipitation hardening. Its hot workability is good and can be extruded into intricate shapes.

Material Resources / Publications

Other Formats Available:

Al-5.9Cu-0.5Mg-0.06Sn

Published: 2015

Al–Cu–Mg alloys are commonly used in aerospace industry and are high strength alloys which can be thermomechanically treated to get different levels of strength and ductility.