Web Content Filters

Filters Applied

No filters

Refine Results

Keyword(s)

MATERIALS RESOURCES

Soldering: Understanding the Basics eBook

Published: 2014
Authors: Mel Schwartz

Covers various soldering methods and techniques as well as the latest on solder alloys, solder films, surface preparation, fluxes and cleaning methods, heating methods, inspection techniques, and quality control and reliability. Geared to scientists, material engineers, designers, manufacturing engineers, and technologists who need immediate practical guidance rather than theoretical instruction.

Material Resources / Publications

Other Formats Available:

Hot Working Guide: A Compendium of Processing Maps, Second Edition eBook

Published: 2015

Hot Working Guide: A Compendium of Processing Maps, Second Edition is a unique source book with flow stress data for hot working, processing maps with metallurgical interpretation and optimum processing conditions for metals, alloys, intermetallics, and metal matrix composites. The use of this book replaces the expensive and time consuming trial and error methods in process design and product development.

Material Resources / Publications

Other Formats Available:

Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference (EPRI 2013)

Published: 2014

Conference proceedings covering the latest technology developments for fossil fuel power plants, including nickel-based alloys for advanced ultrasupercritical power plants, materials for turbines, oxidation and corrosion, welding and weld performance, new alloys concepts, and creep and general topics.

Material Resources / Publications

7075 Al-8v/o C fiber

Published: 2015

Discontinuous fiber reinforced aluminum alloys have high specific strength stiffness and thermal stability and are used for aerospace applications.

Material Resources / Publications

Other Formats Available:

OFHC Copper - 2 ppm Oxygen

Published: 2015

Oxygen free high conductivity (OFHC) copper generally contains less than 50 ppm oxygen.

Material Resources / Publications

Other Formats Available:

OFHC Copper - 11ppm Oxygen

Published: 2015

The conductivity of copper is very sensitive to the oxygen content and copper grades with less than about 50 ppm oxygen are considered to be OFHC grades.

Material Resources / Publications

Other Formats Available:

OFHC Copper - 30 ppm Oxygen

Published: 2015

The hot deformation of OFHC copper is sensitive to the initial grain size since the dynamic recrystallization process nucleates along the prior grain boundaries.

Material Resources / Publications

Other Formats Available:

OFHC Copper - 40 ppm Oxygen

Published: 2015

Hot deformation characteristics of OFHC copper with 40 ppm oxygen was studied by Alder and Phillips using hot compression (see ref. below).

Material Resources / Publications

Other Formats Available:

ETP Copper - 100 ppm Oxygen

Published: 2015

Electrolytic tough pitch (ETP) copper contains oxygen in the range 100 - 650 ppm.

Material Resources / Publications

Other Formats Available:

ETP Copper - 180 ppm Oxygen

Published: 2015

Electrolytic tough pitch (ETP) copper has oxygen content higher than about 100 ppm.