ETP Copper - 220 ppm Oxygen

Published: 2015

This grade of electrolytic tough pitch copper has an oxygen content of 220 ppm which is far in excess of the solubility liquid.

Material Resources / Publications

Other Formats Available:

ETP Copper - 260 ppm Oxygen

Published: 2015

ETP copper with 260 ppm oxygen is of commercial grade and has a high volume fraction of Cu2O particles with a wide range of sizes.

Material Resources / Publications

Other Formats Available:

Copper Powder Compact

Published: 2015

The deformation characteristics of powder metallurgy compacts depends on the technological properties of the powder and the relative density of the compact.

Material Resources / Publications

Other Formats Available:

Cu-3Zn

Published: 2015

Addition of zinc to copper forms brasses which are alpha solid solutions up to about 32% of zinc.

Material Resources / Publications

Other Formats Available:

Cu-10Zn

Published: 2015

Cu-10Zn alloy is an ╬▒ solid solution and is called red brass.

Material Resources / Publications

Other Formats Available:

Cu-15Zn

Published: 2015

Cu-15Zn alloy is called guilding metal and is used as tubes and rods produced by hot extrusion.

Material Resources / Publications

Other Formats Available:

Cu-21Zn

Published: 2015

Cu-21Zn alloy is an alpha solid solution and has a stacking fault energy of about 18 mJ/m2.

Material Resources / Publications

Other Formats Available:

Cu-23Zn

Published: 2015

Cu-23Zn has a stacking fault energy of about 16 mJ/m2.

Material Resources / Publications

Other Formats Available:

Cu-28Zn

Published: 2015

Cu-28Zn has alpha phase structure and has a stacking fault energy of about 15 mJ/m2.

Material Resources / Publications

Other Formats Available:

Cu-30Zn

Published: 2015

The hot deformation characteristics of 70:30 brass are extensively investigated and changes in microstructure are recorded.

Material Resources / Publications

Other Formats Available:

ASM Affiliate Societies