Fabricating Copper Components with Electron Beam Melting

Author: P. Frigola and RadiaBeam, Technologies LLC; O.A. Harrysson, T.J. Horn, H.A. West, R.L. Aman, and J.M. Rigsbee, North Carolina State University; D.A. Ramirez, L.E. Murr, F. Medina, R.B. Wicker, and E. Rodriguez, University of Texas   |   Document Download   |   Product code: ZAMP17207P20

File size: 790 KB

Classified as: Materials Processing and Treatment Materials Properties and Performance

Price: FREE Member price: FREE

The ability to make components from copper and copper alloys via additive manufacturing is spurring a range of novel applications.