ASM International, Materials Park, Ohio, is pleased to announce that Dr. Ursula R. Kattner, FASM, Physical Scientist, National Institute of Standards and Technology, Gaithersburg, Md., is the 2016 J. Williard Gibbs Phase Equilibria Award recipient. She is cited for:
“For contributions to the thermodynamic assessment of metallic alloys and application to metallurgical processing.”
The Gibbs Award was established in 2007 to recognize outstanding contributions to the field of phase equilibria. The award honors J. Willard Gibbs, one of America’s greatest theoretical scientists. Originally proposed by the ASM Alloy Phase Diagram Committee, the award supports ASM’s strong brand identity and reputation in the field of phase diagrams. The J. Willard Gibbs Phase Equilibria Award is endowed by QuesTek Innovations LLC.
In addition to many other contributions, Gibbs laid the thermodynamics foundations of phase equilibria with his brilliant essay, “On the Equilibrium of Heterogeneous Substances”, published in 1876 and in 1878 in the Transactions of the Connecticut Academy.