Controlling matter properties in 2D crystals

By creating atomic chains in a 2D crystal, researchers at Penn State believe they have found a way to control the direction of materials properties in two and three dimensional crystals with implications in sensing, optoelectronics, and next-generation electronics applications.

Whether an alloy has a random arrangement of atoms, or one that is ordered can have large effects on a material’s properties. Nasim Alem, assistant professor of materials science and engineering, and colleagues at Penn State used a combination of simulations and scanning transmission electron microscopy to determine the atomic structure of an ordered alloy of molybdenum, tungsten, and sulfur. They determined that fluctuations in the amount of available sulfur were responsible for the creation of atomic chains of either molybdenum or tungsten.

“We discovered how chains form in a 2D alloy as a result of fluctuations in the amount of a particular precursor, in this case sulfur,” Alem says. “Normally, when we combine atoms of different elements, we don’t know how to control where the atoms will go. But we have found a mechanism to give order to the atoms, which in turn introduces control of the properties, not only heat transport, as is the case in this work, but also electronic, chemical or magnetic properties in other alloy cases. If you know the mechanism, you can apply it to arrange the atoms in a wide range of alloys in 2D crystals across the Periodic Table.”

In the case of the molybdenum, tungsten, and sulfur alloys, the electronic properties were the same in every direction, but simulations were able to predict that the thermal transport properties are smaller perpendicular to the chains or stripes.

“We didn’t know why this crystal forms an ordered structure, so we worked with my Vin Crespi to understand the underlying physics that causes order in this crystal. Our calculations show it was the fluctuations in the third element, sulfur, that was determining how the chains formed,” Alem says.

Vincent H. Crespi, Distinguished Professor of Physics, and professor of chemistry and materials science and engineering who developed the theoretical understanding of the phenomenon, notes that, “Although the interior of the flake is indifferent to whether molybdenum or tungsten occupies any site in the crystal lattice, the edge of the growing crystal does care: Depending on how much sulfur is available at a given location, the edge will prefer to be either 100% molybdenum or 100% tungsten. So as the availability of sulfur randomly varies during growth, the system alternately lays down rows of molybdenum or tungsten. We think this may be a general mechanism to create stripe-like structures in 2D materials.”

Amin Aziz, PhD candidate in Alem’s group, produced the STEM imaging and spectroscopy that shows the fine atomic structure of the alloy samples and their electronic properties.

“When we are able to directly image constitutive atoms of a substance, see how they interact with each other at the atomic level and try to understand the origins of such behaviors, we could potentially create new materials with unusual properties that have never existed,” says Azizi.

A team led by Mauricio Terrones, professor of physics, produced samples of this ordered alloy by vaporizing powders of all three elements, called precursors, under high heat.

Along with Azizi, Terrones, Alem and Crespi, other researchers include Yuanxi Wang, PhD candidate in Crespi’s group, Ke Wang, a staff scientist in the Materials Research Institute who helped with the electron microscopy, PhD candidate Zhong Lin in materials science and Ana Laura Elias, research associate in the Terrones group.

Research support was provided by the National Science Foundation and the U.S. Army Research Office.

Image caption — Electron microscope image of ordered atoms of tungsten and molybdenum against artistic representations of triangular single layer flakes of WxMo1–xS2 on a substrate. Courtesy of Amin Azizi and Andrea Kohler/Penn State.