Heat treatment standards announced for AM metal parts made via powder-bed fusion
February 22, 2018
Source: ASM International
ASTM International, West Conshohocken, Pa., announces F3301 - 18 Standard Specification for Thermal Post-Processing Metal Parts Made Via Powder Bed Fusion. This standard specifies the requirements for thermal post-processing of parts produced via metal powder-bed fusion to achieve the required material properties and microstructure to meet engineering requirements. This standard is intended to be referenced by Material Part Property specifications for powder-bed fusion.
Currently, this standard includes thermal post-processing for the following materials: titanium alloys; cobalt 28 chromium 6 molybdenum; UNS N07718; UNS N06625; UNS 31603; and AlSi10Mg. This specification will be updated as new powder-bed fusion material heat treatments are developed.
https://www.astm.org/Standards/F3301.htm
http://www.astm.org/cgi-bin/resolver.cgi?F3301
Subject Classifications
Materials Processing and Treatment | Additive Manufacturing
Materials Processing and Treatment | Heat Treating
Materials Processing and Treatment | Powder Metallurgy
Materials Processing and Treatment | Thermal Spray Technology