Silver-Aluminum-Magnesium Ternary Alloy Phase Diagram (based on 1939 Haughton J.L.)

Author: Haughton J.L.   |   Document Download   |   Product code: ZAPD-AG-AL-MG-951421

File size: 478 KB

Free to Members

Diagram Type: ternary, vertical section

Concentration range: partial composition; Ag1.2Al17.5Mg81.3-Ag1.2Mg98.8

Temperature: 250.0 - 500.0 °C

Nature of investigation: experimental

Source: ASM Alloy Phase Diagrams Center, 2007; data from Haughton J.L., ALLOYS OF MAGNESIUM. PART IX.-THE CONSTITUTION OF THE MAGNESIUM-RICH ALLOYS OF MAGNESIUM, ALUMINIUM, AND SILVER, J. Inst. Met., Vol. 65, 1939, p 447-456

Reviewed under the auspices of the Alloy Phase Diagram International Commission.

Document includes crystal data for the Silver-Aluminum-Magnesium system, allotropic transformation data, and related references.