Oxygen-Yttrium-Zirconium Ternary Alloy Phase Diagram (based on 1975 Scott H.G.)

Author: Scott H.G.   |   Document Download   |   Product code: ZAPD-O-Y-ZR-208291

File size: 483 KB

Classified as: Binary Systems Cast Irons ...more

Price: $20.00 Member Price: $16.00

Diagram Type: ternary, vertical section

Concentration range: partial composition; Y2O3-ZrO2

Temperature: 0.0 - 3000.0 °C

Nature of investigation: experimental

Remarks: line fixed to make a probable phase diagram

Source: ASM Alloy Phase Diagrams Center, 2011; data from Scott H.G., Phase relationships in the zirconia-yttria system, J. Mater. Sci., Vol. 10, 1975, p 1527-1535

Reviewed under the auspices of the Alloy Phase Diagram International Commission.

Document includes crystal data for the Oxygen-Yttrium-Zirconium system, allotropic transformation data, and related references.