Silicon-Titanium-Zirconium Ternary Alloy Phase Diagram (based on 1995 Salpadoru N.H.)

Author: Salpadoru N.H.; Flower H.M.   |   Document Download   |   Product code: ZAPD-SI-TI-ZR-208317

File size: 522 KB

Price: $20.00 Member Price: $16.00

Diagram Type: ternary, isothermal section

Concentration range: partial composition; Si37.5Ti62.5-Ti-Zr-Si37.5Zr62.5

Temperature: 1200.0 - 1200.0 °C

Nature of investigation: experimental

Remarks: S3-S4 area not clear

Source: ASM Alloy Phase Diagrams Center, 2011; data from Salpadoru N.H., Phase Equilibria and Transformations in a Ti-Zr-Si System, Metall. Mater. Trans. A, Vol. 26, 1995, p 243-257

Reviewed under the auspices of the Alloy Phase Diagram International Commission.

Document includes crystal data for the Silicon-Titanium-Zirconium system, allotropic transformation data, and related references.