Uranium-Zinc Binary Alloy Phase Diagram (based on 1957 Chiotti P.)

Author: Chiotti P.; Klepfer H.H.; Gill K.J.   |   Document Download   |   Product code: ZAPD-U-ZN-905459

File size: 488 KB

Free to Members

Diagram Type: binary phase diagram

Concentration range: full composition; 0-100 at.% Zn

Temperature: 300.0 - 1200.0 °C

Nature of investigation: experimental

Remarks: p= 0.5 MPa

Source: ASM Alloy Phase Diagrams Center, 2007; data from Chiotti P., Uranium-Zinc System, Trans. Am. Inst. Min. Metall. Pet. Eng., Vol. 209, 1957, p 51-57

Reviewed under the auspices of the Alloy Phase Diagram International Commission.

Element concentrations are presented in atomic percent.

Document includes crystal data for the Uranium-Zinc system, allotropic transformation data, and related references.