Vanadium-Zirconium Binary Alloy Phase Diagram (based on 1969 Rudy E.)

Author: Rudy E.   |   Document Download   |   Product code: ZAPD-V-ZR-103669

File size: 110 KB

Classified as: Binary Systems Boilers, Pressure Vessels, and Heat Exchangers ...more

Price: $20.00 Member Price: $16.00

Diagram Type: binary phase diagram

Concentration range: full composition; 0-100 at.% Zr

Temperature: 600.0 - 2000.0 °C

Nature of investigation: experimental

Remarks: melting point of (Zr) ht is inconsistent with established value

Source: ASM Alloy Phase Diagrams Center, 2007; data from Rudy E., Zr-V System, Compendium of Phase Diagram Data, Ternary Phase Equilibria in TM-B-C-Si, E. Rudy, Vol. , 1969, p 75-76

Reviewed under the auspices of the Alloy Phase Diagram International Commission.

Element concentrations are presented in atomic percent.

Document includes crystal data for the Vanadium-Zirconium system, allotropic transformation data, and related references.