Skip to content

The most complex crystal never repeats

The most complicated crystal structure ever produced in a computer simulation is a lesson in how complexity can emerge from simple rules. The icosahedral quasicrystal looks ordered to the eye, but has no repeating pattern. At the same time, it is symmetric when rotated, similar to a soccer ball with five-fold and six-fold patches. Researchers say this property, called icosahedral symmetry, is frequently found on small scales around a single point, like in virus shells or buckyballs—molecules of 60 carbon atoms. But it is forbidden in a conventional crystal.

Like trying to tile a bathroom floor with pentagons, icosahedra do not nicely fill space, says Michael Engel, a research investigator in the chemical engineering department at University of Michigan, Ann Arbor. “An icosahedral quasicrystal is nature’s way of achieving icosahedral symmetry in the bulk. This is only possible by giving up periodicity, which means order by repetition. The result is a highly complicated structure.”

Icosahedral quasicrystals, commonly found in metal alloys, earned the chemist who discovered them more than 30 years ago a Nobel Prize. But engineers are still searching for efficient ways to make them with other materials. Due to their high symmetry under rotation, they can have a property called a photonic band gap, which occurs when the spacing between the particles is similar to that of light. Particles arranged in this way could trap and route light coming from all directions.

“If icosahedral quasicrystals could be made from nano- and micro-meter sized particles, they could be useful in a variety of applications, including communication and display technologies, and even camouflage,” says Sharon Glotzer, professor of chemical engineering.

While these applications are tantalizing, they are very much speculation. Researchers say the most exciting aspect of the findings is the insight they provide into how icosahedral quasicrystals form. “When quasicrystals are studied in the lab, they typically lack direct information about where the atoms are. To figure that out, researchers must look at how the materials scatter light. No one has ever gotten one with icosahedral symmetry to self-assemble thermodynamically in a computer model that is not built by hand, and researchers have been trying for decades,” Glotzer says.

The simulation, which allows researchers to observe how icosahedral symmetry develops for the first time, was done using only one type of particle, which is unique. Typically, two or even three atomic elements are required to achieve a quasicrystal structure. Even though the end product shows long-range order, the particles only interacted with those up to three particle-distances away. When the researchers looked closer, they found that the Golden Ratio governed those interactions.

The Golden Ratio, which is about 1.61, is a mathematically and artistically important number that was first studied by the ancient Greeks. It is related to the Fibonacci Sequence—the simple progression of numbers beginning with 0 and 1 in which the next number is the sum of the previous two—so 0, 1, 1, 2, 3, 5, 8, 13, etc. It is visible in the arrangement of petals in flowers, seeds in a pinecone, branches in trees, and spirals of nautilus shells, for example.

“These findings help answer fundamental questions that are important in all of nature: How do you get really complex arrangements of atoms and molecules from essentially local information? This is a beautiful example of something incredibly rich in structure emerging from very simple rules,” Glotzer says.

The U.S. Army Research Office, the Department of Defense, and the National Science Foundation funded the work.

Image caption — A simulated cross-section of the icosahedral quasicrystal. While the exotic solid has order and rotational symmetry, it does not have a repeating pattern. Courtesy of Michael Engel/University of Michigan.