Skip to content

Hot isostatic press complements state-of-the-art AM center in Florida

A Quintus Technologies hot isostatic press (HIP) will round out the line-up of high-tech equipment in the 10,000-square-foot metal additive manufacturing (AM) center recently opened by Sintavia LLC, in Davie, Fla. The model QIH 15L press gives Sintavia serial production capability for metal parts that meet the exacting quality control standards required by the aerospace and defense industry.

“Without HIP technology, additively manufactured parts are susceptible to porosity and lack of fusion. HIP allows for near 100% net-density parts,” says Sintavia founder Brian Neff, who recognized the promise of AM, also known as 3D printing, during a long career in aviation and parts manufacturing.

The press for Sintavia is equipped with Quintus’s proprietary uniform rapid cooling (URC), which, by incorporating densification and heat treatment in the same equipment, shortens cycle times for higher productivity. The QIH 15L will play a key role in allowing Sintavia’s aviation customers to respond to the mandate to compress build-to-fly time.

The press features a hot zone capability of 7.3 x 19.7 in. (186 x 500 mm), enables pressures up to 30,000 psi (207 MPa), and handles temperatures up to 2550°F (1400°C). Its new modular design shortens installation time and reduces space requirements. It is delivered as a complete unit, with gas compressing system, cooling unit, transformers, electrical cabinets, and pressure vessel all mounted in a 103 x 73-in. skid.

“Quintus HIPs set the industry standard for technology and safety,” says Sintavia co-founder and president Doug Hedges, adding, “While heat treatment is widespread, there is not a lot of HIP capacity available today. As the demand increases, we wanted to stay in front of the curve, controlling our own HIP needs.”

“As one of the first facilities of its kind, Sintavia is at the forefront of the additive manufacturing revolution,” sayss Jan Söderström, CEO of Quintus Technologies. “We are pleased to support their contributions to the aerospace and defense industry.” The press, fully pretested in the Quintus workshop, will be shipped from Västerås, Sweden, in July. It will be commissioned and up and running in September 2016.

“As the AM process continues to penetrate various supply chains, not just aerospace and defense, you’ll see more applications requiring HIP-ing,” says Neff. “For certain very critical parts, HIP will become more or less the standard.”

Image caption — Using high pressure and temperature to improve material performance, the Quintus 15L press features a new modular design that shortens installation time and reduces space requirements.

Facebook
Twitter
LinkedIn