With the advent of nanotechnology, not only can tiny particles be deposited, but the target surfaces or substrates can also be tailored to control the resulting structures.
Researchers at Clarkson University, Potsdam, N.Y., analyzed a model of the process of random sequential adsorption (RSA) and found that even a small imprecision in the position of the lattice landing sites can dramatically affect the density of the permanently formed deposit.
Extreme precision must exist in the pattern of the target surface in order to achieve high perfection and high coverage in the pattern of deposited particles. Researchers compared RSA on three types of surfaces: a continuous (non-patterned) lattice, a precisely patterned surface, and a surface with small imprecisions in the pattern. Very small imprecisions can make RSA proceed as if the surface is continuous. The consequence is that the deposition process is less efficient, and the ultimate coverage is much lower.
In the process of RSA, a continuous surface is covered slowly with a larger fraction of the area remaining uncovered than a precisely lattice-patterned surface. In the past when surfaces on which microscopic particles were deposited were naturally flat (continuous) or had a lattice-structure, the importance of small imprecisions had not been recognized.
Vladimir Privman has been involved in studying aspects of such systems since 2007; however this study, conducted with graduate student Han Yan, was the first to consider the imprecision in the surface lattice-site localization, rather than in the particle size uniformity. Initially suggested by computer modeling, their results were later derived by analytical model considerations which are novel for the research field of RSA.
“The greatest difficulty was to understand and accept the initial numerical finding that suggested results that seemed counterintuitive,” Privman explains. “Once accepted, we could actually confirm the initial findings, as well as generalize and systematize them by analytical arguments.”
Pre-patterned substrates have been studied for applications ranging from electronics to optics, to sensors, and to directed crystal growth. The reported results suggest that efforts at precise fixed positioning and object-sizing in nanomanufacturing might be counterproductive if done as part of forming structures by RSA, under practically irreversible conditions. A certain degree of relaxation, to allow objects to “wiggle their way” into matching positions, may actually be more effective in improving both the density and rate of formation of the desired dense structures, Privman says.
This work has implications that the team is preparing to explore. “Now that we have realized that not only particle non-uniformity, but also substrate-pattern imprecision have substantial effects on the dynamics of the RSA process, we will begin studying various systems and patterning geometries, expanding beyond our original model,” Privman says.