Rolled Alloys, Windsor, Conn., is celebrating 70 years in the thermal processing industry.
The company was founded in 1953 by introducing RA330 as a wrought replacement to cast HT.
Due to RA330’s versatility and availability, it remains the most widely used wrought alloy by commercial heat treaters. Although RA330 exhibits excellent features, there may be better choices for an application. With this being the case, we offer a wide range of heat-resistant alloys to best suit the needs of your application.
Besides this, RA 602 CA is an alloy developed specifically for the highest temperature process, requiring strength and resistance to atmospheres.
One last alloy worth discussing is RA253MA. RA253MA is a lean, heat-resistant stainless steel with high strength and oxidation resistance. With excellent high-temperature properties and low nickel content, RA253MA is a cost-effective material that thermal processors frequently utilize for open-air applications.
https://www.rolledalloys.com/70-years-in-the-thermal-processing-industry/\