NIST and ASM International to Collaborate on Structural Materials Data Demonstration Project

The NIST Material Measurement Laboratory, Gaithersburg, Md., and ASM International, Materials Park, Ohio, through its Computational Materials Data Network, formed a collaboration: the Structural Materials Data Demonstration Project. The project will establish a data repository focused on metallic structural materials, leveraging the overlapping interests and strengths of the two organizations.

27th ASM Heat Treating Society Conference Reports Strong Attendance and a Sold Out Expo Floor

The 27th ASM Heat Treating Society Conference and Exposition (Heat Treat 2013) concluded this week with a strong attendance from the Heat Treating community and a sold out crowd of exhibitors on the show floor. Heat Treat 2013 was held in Indianapolis at the downtown convention center September 16-18. The event attracted over 2000 people from the heat treating community, marking a 16% attendance increase from 2011 and 28% increase from 2009.

Improved hydrophobic materials boost power plant efficiency

Researchers at Massachusetts Institute of Technology, Cambridge, say they found a way to improve the efficiency of steam condensation-the key to worldwide production of electricity and clean water. It has been known for years that making steam-condenser surfaces hydrophobic could improve the efficiency of condensation by causing the water to quickly form droplets. But most hydrophobic materials have limited durability, especially in steamy industrial settings.

Triton receives funding to build fiber-reinforced aluminum production facility

Triton Systems Inc., Chelmsford, Mass., announces that its Composites Division and its partner Specialty Materials Inc., Lowell, Mass., have received MassVentures 2013 START Stage I funding for its FRA Composites technology. FRA (fiber-reinforced aluminum) is a high-strength aluminum alloy randomly reinforced with chopped ceramic (alumina-silicate) fibers. Compared to steel and cast iron, it has equivalent or better resistance to various forms of wear, but is 1/3 the density of ferrous alloys.

Nitrex installs nitriding/nitrocarburizing system at Korean heat treater

Nitrex Metal Inc., Quebec, Canada, has installed a nitriding/nitrocarburizing system at Dongwoo HST Ltd., Korea. Primarily for processing Hyundai ring gears, it includes three Nitreg-based nitriding technologies for a variety of steel types with process recipes for each product application.  Along with the increase in the ring gear business, Dongwoo is expanding to meet the growing demand in Korea for advanced heat treatments with superior capabilities.