New robot boosts solar energy research

Researchers at North Carolina State University, Raleigh, N.C., have created a robot called RoboMapper that can rapidly identify new perovskite materials with improved stability and solar cell efficiency and is capable of conducting experiments more efficiently and sustainably to develop a range of new semiconductor materials with desirable attributes.