Sulzer, Switzerland, with expertise in rotating equipment retrofits and abrasive services, has helped a Philippines petrochemical plant solve a persistent reliability issue and prepare for a 64% increase in capacity by replacing critical pump components with new parts made from high-chromium C6 steel with an abrasion resistant coating applied using a high HVOF process.