Apex Hydraulics, U.K., has developed a Corex tungsten chromium carbide thermal spray coating that provides hardness up to 1400 HV and bond strength of about 10,000 psi.
Ceramic coating reduces temperature on innovative superboat
The aeroacoustics of jets
Simulations helps scientists understand and control turbulence in humans and machines illustration showing air pushed through vocal folds causing them to vibrate.
Embedding quantum dots aids in anticounterfeiting
Quantum Materials Corp., San Marcos, Tex., secured 3D printing and additive manufacturing anticounterfeiting quantum dot detection technology developed at Virginia Tech, Blacksburg.
Spectris acquires La Corp. Scientifique Claisse Inc.
Spectris plc in Surrey, England, (LSE: SXS), the productivity-enhancing instrumentation and controls company, announced on June 23 that it acquired the business and assets of the Canadian company La Corp. Scientifique Claisse Inc., a global market leader in sample preparation for atomic spectroscopy (including x-ray) analysis, for an undisclosed sum. Revenues for the year ending March 2014 were CAD 13 million.