Bruker Corp., Billerica, Mass., has formed an official partnership with the University of Manchester’s National Graphene Institute (NGI).
Edax launches new XRF analyzers for coating thickness and composition analysis
TSMC certifies Mentor Graphics tools for TSMC 10nm FinFET Technology
Multi-sensor microscope optical head enables multiple FA techniques
Quantum Focus Instrument Corp., Vista, Calif., introduces QuantumScope, a multi-sensor microscope optical head in which mid-wavelength infrared hot-spot detection, photoemission, and laser signal injection microscopy techniques are integrated into the same optical inspection platform.