Diffusion and temperature: Water, pen ink, and vinegar

Watch how pen ink diffuses in two cups of water: One with cold water and the other with hot. The pen ink is not visible in the hot water glass while the cold water glass looks purple/blue. Add vinegar and watch what happens!

Replacing stainless steel?

HAM-LET, UK, a leading global manufacturer of instrumentation valves and fittings for industrial and high purity applications, launched PuRight—a new, enhanced stainless steel 316L material at Semicon West earlier this month.

New metamaterial gives light a one-way ticket

Researchers at the National Institute of Standards and Technology (NIST), Gaithersburg, Md., built a silver, glass, and chromium nanostructure that can all but stop visible light cold in one direction while giving it a pass in the other.

Hollow-fiber MOF membranes could cut energy use

Researchers at Georgia Institute of Technology, Atlanta, developed a microfluidic technique for fabricating a new class of metal-organic framework (MOF) membranes inside hollow polymer fibers that are just a few hundred microns in diameter.

Notre Dame and General Electric to collaborate on gas turbine R&D facility

The University of Notre Dame, South Bend, Ind., and General Electric Power & Water, Schenectady, N.Y., announce plans to work together to build a $36 million research and test facility with the goal of making better massive gas turbines used by aircraft, power plants, and the oil and gas industry.