Using metallic osmium (Os) in experimentation, an international group of researchers demonstrated that ultra-high pressures cause core electrons to interplay, which results in experimentally observed anomalies in the compression behavior of the material. Os is one of Earth’s most exceptional elemental materials, possessing the highest known density at ambient pressure, one of the highest cohesive […]