Asylum Research, Santa Barbara, Calif., an Oxford Instruments company, has developed Scanning Microwave Impedance Microscopy (sMIM), an atomic force microscopy technique that enables nanoscale mapping of permittivity and conductivity.
Lasertec U.S.A., San Jose, Calif., introduces the WASAVI Series BGM300. This instrument measures silicon wafer thicknesses and TSV depths prior to back grinding 3D semiconductor devices.
Bruker Nanosurfaces Division, Billerica, Mass., introduces the Dektak XTL Stylus Profiler, extending its stylus profilometry capabilities to 200 and 300 mm semiconductor wafer fabs and next-generation touch panel manufacturers.
Semiconductor Research Corporation (SRC), Research Triangle Park, N.C., has launched a new initiative on Trustworthy and Secure Semiconductors and Systems (T3S).