Researchers at NIST, the University of Maryland, Cand Sandia National Laboratories, imaged the inner workings of experimental solid-state batteries as they charged and discharged while making detailed measurements of their electrochemical health.
SSAB Steel, Sweden, has launched the new Hardox Tube 500 family, which provides the same hardness and toughness as Hardox wear plate, but in circular form.