Seco Warwick, Meadville, Pa., introduces UniCase Master, a single flow, precision case-hardening system said to reduce distortion in gears; and the ZeroFlow gas nitriding process.
MTS provides test equipment to engineering lab at Penn State
Constellium launches Aeral aluminum for aerosol cans
Constellium N.V., Amsterdam, has launched Aeral, an aluminum solution designed for making aerosol containers by the “drawn and ironed” technology currently used to produce beverage cans.