The NASA Michoud Assembly Facility in New Orleans announces that engineers have welded together the first two segments of the Orion crew module that will fly atop NASA’s Space Launch System rocket on a mission beyond the far side of the moon.
Contour Hardening Inc., Indianapolis, the developer of patented Micropulse induction heat treating technology, announces the recent ISO/TS 16949:2009 certification of its heat treating service facility in Guanajuato, Mexico.