NASA Langley recognized for advancing helicopter research

NASA Administrator Charles Bolden was at NASA’s Langley Research Center, Hampton, Va., on May 8 to participate in a ceremony recognizing Langley’s decades of contributions to improving helicopters and other vertical flight aircraft.

Technique creates stronger carbon nanotube films

Researchers developed an inexpensive technique called “microcombing” to align carbon nanotubes (CNTs), which can be used to create large, pure CNT films that are stronger than previous films.