Ipsen, Cherry Valley, Ill., has expanded its services to include calibration and survey services that adhere to strict Nadcap requirements.
New XRD system combines Turbo X-ray source, Eiger photon detector, Atlas goniometer
Bruker AXS, Billerica, Mass., announces that its new D8 Discover Plus X-ray diffraction system combines the high power of the TXS-HE high-efficiency Turbo X-ray Source, with the large detection area and dynamic range of the Eiger2 R 500K multi-mode hybrid photon counting detector, and the high-endurance Atlas goniometer.