Limiting the impact of technology on materials extraction

A team of researchers from the University of Exeter, Minviro, the British Geological Survey, and the Circular Economy Solutions Unit has shown the benefits of utilizing a life cycle assessment (LCA) in the quest to enhance ‘green’ mining techniques.

New high-entropy alloys with attractive hydrogen storage properties

A group of materials and computer scientists from Sandia National Laboratories collaborated with a few international researchers to create 12 new alloys over the course of more than a year. The study shows how machine learning can help expedite the future of hydrogen energy by enabling the simple creation of hydrogen infrastructure for consumers.

TMC – The Future of Metallurgy

The Metals Company (TMC) is launching a processing pilot campaign to convert seafloor nodules into an alloy that contains metals critical in the production of batteries. Their custom process starts with polymetallic nodules and ends with battery-grade metals, such as nickel, sulfate, cobalt sulfate, and copper. Their goal is to have a metallurgical processing plant […]