Team examines operating limits in solid-state batteries to improve range of EVs

A collaboration among researchers at Vanderbilt University (Nashville, Tenn.), the University of Pennsylvania, (Philadelphia), the Advanced Photon Source, (Lemont, Ill.), and Toyota Research Institute North America (TRINA), a division of Toyota Motor North America R&D (Ann Arbor, Mich.), examined operating limits and failure mechanisms in a family of solid-state batteries based on thiophosphate materials.