H.C. Starck, Newton, Mass., introduces the Ultra 76 Plus tantalum alloy, which is designed to combat aggressive hazardous-chemical corrosion in hot concentrated acids.
Plansee, Austria, recently invested in an ultramodern cold rolling mill to produce thin and medium-thickness molybdenum sheets up to 1000 mm wide, and to ensure increased capacity.
Constellium N.V., Amsterdam, announces that it has formed a partnership with Stelia Aerospace and CT Ingenierie to optimize large aluminum aerostructures via additive manufacturing.