NIST scientists build a better nanoscale LED

A new design for light-emitting diodes (LEDs) developed by a team of scientists at the National Institute of Standards and Technology (NIST), Gaithersburg, Md., may hold the key to overcoming a light source’s long-standing efficiency limitation.

The science of forging

This video from Real Engineering explains the science of forging metals. By describing differences in crystal structure. and the influence of temperature on the microstructure, the video lucidly illustrates how metals react on forging.