Copper’s Conductivity and Antimicrobial Properties Inspire Renewed Interest

There is a growing interest in copper’s antimicrobial benefits for surface applications to possibly reduce the spread of COVID-19. In this digital-first article from Advanced Materials & Processes, ASM International’s flagship magazine, Harold T. Michels, consultant and retired senior vice president, Copper Development Association, Manhasset, N.Y., details the antimicrobial features of copper and its alloys. Paired with his research is a review of the metal’s other properties, which make it suitable for a range of uses. With content based on the peer-reviewed, internationally revered ASM Specialty Handbook: Copper and Copper Alloys, this article provides vital information to consider when determining whether to use copper for an application.