In the biggest infrastructure project ever, Italy has begun the MOSE Project (MOdulo Sperimentale Elettromeccanico). Due for completion in 2016, the goal is to build massive movable gates to protect the city of Venice from the encroaching Adriatic Sea during high tides.
How heat treatment affects Nitinol wires
Lumenous provides laser micro-machining for tube and sheet
Lumenous Device Technologies, Sunnyvale, Calif., provides laser-micromachining and premium finishing to the medical device and precision instrument industries worldwide.
Shape Memory and Superelasticity: Advances in Science and Technology
The new journal, Shape Memory and Superelasticity: Advances in Science and Technology, now has articles to view online.