Researchers of the Paul Scherrer Institute in Switzerland have reportedly made detailed 3-D images of a commercially available computer chip, marking the first time a nondestructive method has visualized the paths of a chip’s internal 45-nm-wide wiring and its 34-nm-high transistors clearly without distortions or deformations.