The graph shows the time-temperature-transformation (TTT) curve for an unstabilized 430-type alloy with carbon plus nitrogen of 0.08%.

Juno Visits Jupiter

On July 4, NASA’s Juno spacecraft, about the size of a bus, entered orbit (about 3100 miles from the surface) around the gas giant Jupiter, which is 1.76 billion miles from Earth.

Shape-memory polymers exhibit triple shape-memory behavior

Oak Ridge National Laboratory, Tenn., reports that a team of researchers from ORNL, Washington State University, and the University of Idaho, have developed shape-memory polymers that exhibit triple-shape-memory behavior, meaning that the polymers can transform from one temporary shape to another at one temperature, and then back to a permanent shape at a different temperature.