Printing furniture with liquid metal
Researchers at the Massachusetts Institute of Technology (MIT) in Cambridge, Massachusetts, have developed an additive manufacturing technique that can print rapidly with liquid metal, producing large-scale aluminum parts, like table legs and chair frames, in a matter of minutes. MIT’s Self-Assembly Lab research team includes Zain Karsan, Kimball Kaiser, Jeremy Bilotti, Bjorn Sparrman, Schendy Kernizan, […]